Type of powder material |
WC-CoCr Cobalt-chromium tungsten carbide composite powder 86/10/4 Reunion sintering |
brand(PZ) |
PZ-603 |
specifications(um) |
30/5 38/10 45/15 53/20 |
Performance and application |
APS, HVOF, HVAF fine grained tungsten carbide The maximum operating temperature 500 ℃ CoCr has better corrosion resistance than Co the coating is hard and dense, resistant to sliding wear and erosion wear for paper rollers, valves and pin valves, hydraulic cylinders, compressor shafts, landing gear, etc. |
W | Balance |
Cr₂0₃ | 3.5-4.5 |
C | 5.0-5.5 |
Co | 9.0-11.0 |
Fe₂0₃ | N.R. |
Others | 1.0MAX |
Product | Nominal Size Distribution(um) |
WC-CoCr | -53+20 |
WC-CoCr | -38+10 |
WC-CoCr | -45+15 |
jacket | turbocharger |
Part function:The engine set can be made of light materials | Part function:Boost engine |
Matrix material:Cast iron | Matrix material: Cast aluminum silicon alloy or all kinds of cast iron |
Function of the coating:Reduce gasoline and fuel consumption | Function of the coating:Reduce gasoline and fuel consumption |
Process technology: Atmospheric plasma spraying |
Process technology: Atmospheric plasma spraying |